Activated Alumina Balls
Molecular Formula: Al2O3 • nH2O (0<N≤0.8)
Activated alumina has much micro-paths, so the specific surface is large. It can be used as absorbent desiccant and catalyst carrier. It is also a kind of trace water desiccant and the pole-molecular absorbent, according to the absorbed molecular polarization, the attachment force is strong for water, oxide, acetic acid, alkali etc.
This product is used for deep drying of gas or liquid phase of petrochemicals and adsorption drying by automatic instruments.
Technical Data:
Items |
DS401 |
DS402 |
DS403 |
DS404 |
DS405 |
|
Appearance |
White, Sphere, No Odor, Insoluble In Water, Innocuous |
|||||
Crystal Type |
x-p |
x-p |
x-p |
x-p |
x-p |
|
Chemical Composition |
Al2O3% |
≥93 |
≥93 |
≥93 |
≥93 |
≥93 |
Na2O % |
≤0.3 |
≤0.3 |
≤0.5 |
0.15-0.3 |
≤0.3 |
|
LOI |
% |
6-8 |
6-8 |
≤8 |
≤5 |
6-8 |
Bulk Density |
g/ml |
0.68-0.72 |
0.70-0.75 |
0.65-0.75 |
0.70-0.80 |
0.68-0.72 |
Surface Area |
m2/g |
≥300 |
≥300 |
250-280 |
≥280 |
≥350 |
Pore Volume |
ml/g |
0.30-0.45 |
0.30-0.42 |
0.40-0.46 |
0.40 |
0.30-0.50 |
Static Absorption (RH=60%) |
% |
Water Absorption |
Fluorine Absorption |
Water Absorption |
Water Absorption |
Water Absorption |
Active |
% |
|
|
56-62 |
|
|
Attrition Loss |
% |
≤1.0 |
≤1.0 |
≤1.0 |
≤0.4 |
≤0.8 |
Crushing Strength (N/Particle)
|
0.4-1.2 |
|
≥30 |
|
|
|
1-2 |
≥40 |
≥40 |
|
|
|
|
2-3 |
≥60 |
≥60 |
|
|
|
|
3-5 |
≥100 |
|
≥100 |
≥100 |
≥100 |
|
4-6 |
≥120 |
|
≥130 |
≥120 |
≥110 |
|
5-7 |
≥160 |
|
|
|
|
|
6-8 |
≥180 |
|
|
|
|
SW401: is for as adsorbent
SW402: is for defluorinating
SW403: is for absorption in producing hydrogen perixide (H2O2)
SW404: is for catalyst carrier
SW405: is for dehydrating and drying in air seperation etc.
Packing:
25kg/Bag
150kg/Steel Drum
Other packing according to your requirement.
Instruction: Prevent alumina driers from exposing directly to the air.
Waring: Alumina driers adsorption activity is an exothermic reaction, any contact to human body is dangerous.